| Fasteners and Hardware | Bolts, nuts, screws, washers, clips, and stamped hardware | Carbon steel, stainless steel, alloy steel, and copper alloys | 650–900°C | Nitrogen, endothermic gas, or controlled air depending on the material | Continuous loading, strong temperature uniformity, durable mesh belt, and adjustable belt speed | Hardness, tensile strength, decarburization, oxidation, and dimensional stability |
| Automotive Components | Stamped parts, clips, springs, brackets, small gears, and precision fittings | Low-carbon steel, medium-carbon steel, stainless steel, and spring steel | 600–850°C | Protective nitrogen-based atmosphere or controlled endothermic gas | Multi-zone heating, accurate atmosphere control, low distortion, and automated temperature recording | Mechanical strength, surface condition, fatigue performance, and repeatability |
| Bearing and Precision Mechanical Parts | Small rings, cages, rollers, sleeves, and precision-machined components | Bearing steel, high-carbon chromium steel, and alloy steel | 650–850°C | High-purity nitrogen or another low-oxidation protective atmosphere | Low-temperature deviation, stable conveyor movement, clean furnace chamber, and controlled cooling | Hardness uniformity, dimensional accuracy, residual stress, and surface oxidation |
| Copper and Copper-Alloy Processing | Strips, wires, terminals, connectors, tubes, and stamped electrical parts | Copper, brass, bronze, and copper-nickel alloys | 350–750°C | Nitrogen, hydrogen-nitrogen mixture, or vacuum-compatible protective conditions | Fast heat transfer, non-contaminating belt materials, precise cooling, and oxidation prevention | Electrical conductivity, elongation, surface color, softness, and dimensional consistency |
| Electrical and Electronic Components | Metal terminals, contact parts, connector components, shielding pieces, and small assemblies | Copper alloys, nickel alloys, stainless steel, and plated metals | 300–800°C | Dry nitrogen or another clean protective atmosphere compatible with coatings | Clean chamber design, precise atmosphere flow, low particle generation, and gentle conveying | Contact resistance, coating adhesion, surface cleanliness, and dimensional accuracy |
| Powder Metallurgy | Sintered gears, bushings, structural parts, and small wear-resistant components | Iron-based, stainless-steel, copper-based, and nickel-based powder materials | 700–1,150°C | Hydrogen-nitrogen, nitrogen, dissociated ammonia, or endothermic gas | High-temperature belt construction, controlled gas flow, staged heating, and reliable cooling zones | Density, carbon potential, dimensional change, porosity, strength, and surface condition |
| Wire, Cable, and Metal Strip | Metal wire, flat strip, spring wire, electrical conductor, and drawn products | Carbon steel, stainless steel, copper, brass, and nickel alloys | 400–950°C | Nitrogen, hydrogen-nitrogen, or controlled reducing atmosphere | Stable tension control, continuous feed-through design, uniform heating, and oxidation protection | Tensile strength, elongation, surface finish, conductivity, and coil-to-coil consistency |
| Tool and Blade Manufacturing | Cutting blades, saw components, small tools, punches, and wear-resistant parts | Tool steel, stainless steel, high-speed steel, and hardenable alloy steel | 650–900°C | Vacuum-compatible or protective nitrogen-based atmosphere, depending on the process | Accurate temperature control, low distortion, programmable recipes, and controlled cooling | Hardness, toughness, straightness, edge quality, and microstructural uniformity |
| Metal Stamping and Forming | Stampings, drawn parts, brackets, covers, and formed sheet-metal components | Low-carbon steel, stainless steel, aluminum alloys, and copper alloys | 250–850°C | Air, nitrogen, or low-oxidation atmosphere selected according to the alloy and surface requirements | Flexible belt speed, even product spacing, rapid recipe changes, and low-temperature overshoot | Formability, hardness, springback, surface appearance, and part distortion |
| Medical and Laboratory Hardware | Small surgical instruments, fittings, clips, dental components, and laboratory parts | Stainless steel, titanium alloys, cobalt-chromium alloys, and specialty metals | 500–1,050°C | High-purity inert or protective atmosphere selected for the specific alloy | Cleanable construction, traceable process records, precise control, and low contamination risk | Corrosion resistance, cleanliness, hardness, dimensional accuracy, and batch traceability |
| General Heat-Treatment Services | Mixed small metal parts requiring stress relief, softening, or recrystallization annealing | Carbon steel, stainless steel, copper alloys, aluminum alloys, and nickel alloys | 200–1,100°C | Air, nitrogen, inert gas, or reducing atmosphere based on the material and finish | Wide operating range, modular heating zones, recipe storage, easy maintenance, and adaptable loading systems | Temperature uniformity, hardness, surface oxidation, throughput, and energy consumption |